The castability, mechanical properties, and fracture characteristics of Ti-15Mo-5Zr-3Al alloy were compared with those of Ti-6Al-7Nb alloy and pure titanium (CP Ti) for application of this β-type titanium alloy in cast dental prostheses. Cast specimens were prepared with a centrifugal casting machine. A tensile test was performed according to ISO standard 22674. The castability index for Ti-15Mo-5Zr-3Al was lower than those for Ti-6Al-7Nb and CP Ti. The tensile strength of Ti-15Mo-5Zr-3Al was 852 MPa, which was lower than that of Ti-6Al-7Nb and higher than that of CP Ti. The proof strength of Ti-15Mo-5Zr-3Al was 799 MPa, which was comparable to that of Ti-6Al-7Nb and higher than that of CP Ti. The elastic modulus of Ti-15Mo-5Zr-3Al was 81.0 GPa, which was lower than the values for Ti-6Al-7Nb and CP Ti. Elongation of Ti-15Mo-5Zr-3Al was 5.1%, which was comparable to that of Ti-6Al-7Nb and less than that of CP Ti. The shape of the fractured segment was narrower for Ti-15Mo-5Zr-3Al than for Ti-6Al-7Nb and CP Ti. The deformation characteristics of Ti-15Mo-5Zr-3Al may result in decreased stress relative to increased strain during plastic deformation in the stress-strain diagram. In conclusion, Ti-15Mo-5Zr-3Al alloy has a low elastic modulus and exhibits limited ductile plastic deformation in cast dental prostheses.
No takes yet. Share an insight, caveat, or question.
Koizumi et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: