A laser interferometer was used to measure the d33 piezoelectric coefficient of wurtzite GaN. The GaN was in the form of 1 μm thick films, grown by chemical vapor deposition and the measurement of the piezoelectric coefficient was made with a spatial resolution of 100 μm. Sample mounting was found to play an important part in the observed response. For rigidly mounted samples, the measured d33 was 2.0±0.1 pm V−1.
No takes yet. Share an insight, caveat, or question.
Muensit et al. (1998) studied this question.