Overcoming the strength-ductility trade-off remains a daunting challenge for titanium (Ti) industry. Duplex ( α + β ) Ti alloys, represented by Ti-6Al-4 V, are the mainstay of Ti industry. However, the poor deformability of hexagonal close-packed (HCP) α phase, combined with semi-coherent α / β boundaries for strain incompatibility often cause limited elongation. Here, we propose an innovative strategy that harnesses O atoms with strong hardening ability in Ti alloys, as well as the rapid cooling and highly thermal gradients of laser powder bed fusion to construct a duplex Ti alloy, involving HCP Ti matrix embedded with O-rich nano-coherent face-centered cubic (NC-FCC) Ti. The duplex Ti-0.615 wt% O alloy achieves a high ultimate tensile strength of 1020 ± 4 MPa and an exceptional elongation of 21.8 ± 0.5%, together with a superior specific strength-ductility product of 4.93 GPa·%·cm 3 ·g − 1 . This unprecedented combination of mechanical properties originates from the O-rich NC-FCC, which promote dislocation slip transfer across the coherent phase boundaries (CPBs) and formation of extensive stacking faults near CPBs for enhanced strain compatibility. Additionally, the O-rich NC-FCCs strengthen the alloy via solid solution strengthening from O atoms. This work opens a promising avenue towards a new generation of lightweight high-performance metallic materials through customized phase engineering induced by interstitial atoms.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Yu et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: