Step-shaped (110) oriented silicon wafers are oxidized in dry O2 (900–1150°C) and the cross sectional views of oxide are observed by scanning electron microscopy. At lower temperature (900–950°C), the oxide thickness at te edge the reduced compared to the other regions, but the reduction cannot be observed at higher temperatures (1000–1150°C).