Answers are grounded in this paper and cite their sources.
The most important ferroelectric properties of the system Pb(Sc0.5Nb0.5)1–xZrxO3 were measured as a function of temperature. With increasing Zr concentration the system approaches more closely Curie-Weiss behaviour. Tails that exist above the transition temperature in the spontaneous polarization versus temperature curves tend to disappear as more Zr is added to the system. The ferroelectric transition becomes more first-order-like as the concentration of Zr is increased. Above x = 0.85 the system becomes antiferroelectric. Our work clearly demonstrates for the first time that it is possible to change continuously from a “diffuse” to a “sharp” transition while ferroelectricity is maintained.
No takes yet. Share an insight, caveat, or question.
Kuchar et al. (1971) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: