In this study, Zn–W films were developed on 316L stainless steel via chronopotentiometric electrodeposition to improve its protective performance. Zinc was employed for its ability to form a passive layer, while tungsten was incorporated to enhance mechanical strength and durability. A citrate-based electrolyte was used to facilitate co-deposition, overcoming the challenges of direct tungsten electrodeposition. Deposition was conducted within a current density range of −35 to −50 mA cm−2, as identified from cyclic voltammetry. X-ray diffraction confirmed the formation of hcp Zn–W phase with crystallite sizes of 15–22 nm, indicating microstructural refinement due to tungsten incorporation. The resulting films exhibited a smooth, compact and flower-like morphology. Energy-dispersive spectroscopy (EDS) analysis indicated that the coatings were predominantly Zn-rich, with a maximum Zn content of ∼97.62 wt.% obtained at −35 mA cm−2. At higher current densities, the Zn content decreased slightly, while the maximum tungsten incorporation reached ∼3.28 wt.%. The coatings exhibited an average thickness of ∼ 1.5 µm, confirming the formation of a uniform and continuous layer over the substrate. Open-circuit potential measurements indicated passive layer formation. Tafel analysis showed the highest polarisation resistance (Rp) of 223 Ω cm² at −35 mA cm−2.
No takes yet. Share an insight, caveat, or question.
Singh et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: