Answers are grounded in this paper and cite their sources.
A study has been made of graft copolymerization of methyl methacrylate onto native potato starch in aqueous slurry at 30°C. As Mn3+ concentration was increased from 0.15 X 10‐3M to 1.0 X 10‐3M, conversion of monomer to polymer and add‐on of polymer to starch increased and frequency of grafts (anhydroglucose units per grafted chain) decreased sharply. The average molecular weights of the PMMA grafts also decreased in this range. At Mn3+ concentrations from 1.0 X 10‐3M to 3.0 X 10‐3M, only minor changes in grafting parameters were observed. When the amount of starch charged per batch was increased threefold, the add‐on decreased sharply, the molecular weight increased slightly, and the conversion of MMA monomer to polymer remained almost constant. The increase in frequency of grafts (AGU/chain) was almost directly proportional to the increase in the amount of starch charged. In all cases the average molecular weights of grafts were of the order of 106 and the grafting efficiencies high, normally greater than 85%. These results were compared with those previously obtained for grafting of acrylonitrile onto starch. They were interpreted in terms of initial (Mn3+)/(AGU) ratio, total number of radicals initiating grafting, and compatibility of methyl methacrylate monomer with poly(methyl methacrylate) chains.
No takes yet. Share an insight, caveat, or question.
Mehrotra et al. (1978) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: