Molybdenum oxide films offer a rich variety of properties for diverse applications, but exclusive synthesis of desired phases is a major challenge. Here, we demonstrate that oxygen flow ratio fO2 = [O2]/[Ar + O2] is crucial not only for phase selection of non-layered monoclinic MoO2 and layered orthorhombic α-MoO3 but also for controlling grain size and preferred orientation. Both mica and sapphire support exclusive MoO2 formation for 0.15 ≤ fO2 ≤ 0.25 at deposition temperatures Tdep = 400 and 500 °C, while α-MoO3 forms only at Tdep = 400 °C for 0.35 ≤ fO2 ≤ 0.5. Within the fO2 windows favoring each phase, high fO2 fosters large grains with out-of-plane 0k0 texture, except for MoO2 on c-sapphire at Tdep = 500 °C, where no fO2-texture correlation is discernible. These findings provide a framework for rational synthesis of single-phase monoclinic MoO2 and orthorhombic MoO3 with control over texture and microstructure to access desired properties.
No takes yet. Share an insight, caveat, or question.
Lahiji et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: