The development of high-performance electrochemical energy storage systems is highly desirable for portable and wearable electronic devices. In this study, we proposed a new method to prepare a yolk–shell NiMoO 4 /V 2 CT x @reduced graphene oxide (rGO) composite material using a room-temperature ionic liquid (RTIL)-assisted hydrothermal method. NiMoO 4 was incorporated into the V 2 CT x MXene layer in the presence of the RTIL 1-butyl-3-methylimidazole tetrafluoroborate ([Bmim]BF 4 ). rGO was coated on the NiMoO 4 /V 2 CT x yolk under electrostatic forces. [Bmim]BF 4 effectively prevents the overoxidation of V 2 CT x MXene during the hydrothermal synthesis of NiMoO 4 and reduces its surface energy, which makes the NiMoO 4 /V 2 CT x @rGO composite highly stable. This alternating arrangement facilitates the rapid diffusion and transport of electrolyte ions, resulting in excellent electrochemical performance of the NiMoO 4 /V 2 CT x @rGO composites. Bamboo-shaped MoO 2 @Fe 2 O 3 /N-doped carbon (NC) was used as a negative electrode material to assemble a solid asymmetric supercapacitor (ASC) with NiMoO 4 /V 2 CT x @rGO (NiMoO 4 /V 2 CT x @rGO//MoO 2 @Fe 2 O 3 /NC). The ASC possesses a high energy density of 56.1 W h kg –1 at 800 W kg –1 . The capacitance retention rate remains as high as 90.7% after 5000 cycles, demonstrating that the proposed material has promising performance for supercapacitor applications.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: