Corrosion rates of iron in chromate and nitrite solutions were measured by a sensitive electric resistance method supplemented by weight loss. The critical concentration below which corrosion increases or pitting occurs is for and for . Presence of Cl − and increases these values. Sulfates break down passivity in nitrite solutions more so than do chlorides; the reverse is true of chromate solutions. Minimum concentration of passivator to avoid pitting in presence of Cl − or follows the relation where and are molarities of salt and passivator respectively. In chromate solutions in the alkaline range of p H, the corrosion rate is low (0.08 mdd) and no pitting occurs. In the acid range, corrosion remains low to at least p H 2.8 provided is used to adjust p H; when is used instead, the corrosion rate increases below p H 5 and pitting begins at p H 3. At temperatures up to 100°C, the steady‐state corrosion rates in chromates remain low (<0.1 mdd). An initial higher rate precedes the final lower rate. These relations are explained by passivation through anodic polarization and competitive adsorption of Cl − or with the passivator ion for a site on the passive film. The data support the view that adsorbs more strongly than does .
No takes yet. Share an insight, caveat, or question.
Matsuda et al. (1964) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: