Answers are grounded in this paper and cite their sources.
The magnetic after-effect, observed as a time decrease of the initial susceptibility, has been measured in high-purity, neutron-irradiated iron. Integrated doses varied from 1.1 × 1017 to 1.1 × 1019 neutrons cm−2 (E > 0.1 MeV) and the irradiation temperature was about 80 °C. Strong relaxation peaks were observed at −65 and −15 °C; these have been analysed quantitatively and interpreted as being due to the reorientation of interstitial-impurity clusters and to impurity interstitials. Above 0 °C a relaxation peak occurs at 70 °C which is complicated by the occurrence of an annealing process. This peak is attributed to an impurity-vacancy cluster. The relaxation peaks anneal out between 70 and 200 °C. This is attributed to the migration of vacancies and vacancy-impurity clusters. During the annealing of these relaxation peaks another relaxation peak below −150 °C is built up which is identified with the cold-work peak of hydrogen atoms which have been detrapped from defect clusters during the annealing process.
No takes yet. Share an insight, caveat, or question.
Blythe et al. (1971) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: