Answers are grounded in this paper and cite their sources.
Metal-semiconductor-metal ultraviolet (UV) photodetectors were created with zinc-oxide colloidal nanoparticles coated with polyvinyl-alcohol. Gold-interdigitated finger contacts with different parameters were patterned on the nanoparticles by optical lithography. The photodetectors exhibited UV-photogenerated current to dark current ratios ranging from 3.85 × 106to 1.34 × 108, depending on the finger parameters. The spectral responses demonstrate a 375 nm cutoff wavelength, with a peak responsivity of 731.42 A/W at 345 nm.
No takes yet. Share an insight, caveat, or question.
Qin et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: