We devised an effective method of deposition of photocatalytic WO 3 films for the decomposition of volatile organic compounds. Amorphous WO 3 films were deposited on unheated fused silica glass substrates by reactive DC magnetron sputtering with a W metal target, followed by crystallization through annealing at 300–800 °C in air. Under visible light irradiation, a film annealed at 400 °C proved significantly more effective than a WO 3 film crystallized during deposition on a heated (800 °C) substrate for achieving photocatalytic decomposition of CH 3 CHO. Even more remarkable photocatalytic results were obtained for a film that was loaded with Pt nanoparticles after postannealing.