Answers are grounded in this paper and cite their sources.
This study assessed the effect of surface conditioning methods and ceramic primers on the repair strength of resin-composite to zirconia-veneering ceramic with different defect sizes. Zirconia (IPS e.max ZirCAD) (n = 30) and veneering ceramic (Creation) (n = 30) alone acted as control groups. In the 1st part of the study, zirconia was silica-coated (SC) and treated with 3 different ceramic primers (Monobond Plus + Helibond (MBP), Clearfil Ceramic Primer Plus (CCP), Z-Prime Plus (ZPP)). Feldspathic ceramic was etched with 9.6% hydrofluoric acid (HF) and primed. After repairing with resin-composite (Empress Esthetic) and testing for shear bond strength (SBS), the best performing adhesive system (MBP) for both substrates (N = 60, n = 10 per group) was tested for defect sizes of (a) 3.2, (b) 4, (c) 5 mm with zirconia (diameter: 1.7 mm) being in the center (N = 60, n = 10 per group). Half of the specimens were repaired employing HFSC and the other half with SCHF. The specimens were stored in distilled water (37 °C, 24 h) and thermocycled (5–55 °C, 5000 cycles). The resin-substrate interface was loaded under shear force (1 mm/min). Data (MPa) were analyzed using two-way ANOVA and Tukey’s tests (α = 0.05). In the 1st study, MBP resulted in significantly higher SBS (MPa) for both zirconia and veneering ceramic (Zirconia: 14.2 ± 3.6; Veneer: 11.0 ± 3.7), compared to those of CCP (Zirconia: 9.4 ± 2.2; Veneer: 7.5 ± 3.4) and ZPP (Zirconia: 5.0 ± 0.9; Veneer: 5.9 ± 2.1) (p < 0.01). Neither the size of the defect (p > 0.05) nor repair sequence showed a significant effect (p > 0.05) on the repair bond strength with mainly mixed type with cohesive fracture in the veneering ceramic.
No takes yet. Share an insight, caveat, or question.
Schellenberg et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: