The facile desorption of C 8 and heavier products from solid acid alkylation catalysts is essential to thwart catalyst deactivation by fouling. To better understand this phenomenon, a tapered element oscillating microbalance (TEOM) was employed to investigate the adsorption/desorption characteristics of 224-trimethylpentane (224-TMP), a proxy C 8 alkylate product, on β-zeolite and mesoporous materials ( T = 298−473 K, P 224-TMP = 0−0.3 bar). It is found that the 224-TMP desorption rates from saturated β-zeolite (by helium purging) are characterized by a rapid initial “burst” of 224-TMP followed by a rather long desorption phase. Complementary experimental and modeling investigations using pelletized β-zeolites of known sizes indicate that the adsorption rate and initial desorption (during the burst phase) rate of 224-TMP are controlled by meso-/macropore diffusion resistance external to the β-zeolite crystals and that the long transient could be due to pore diffusion resistance within the β-zeolite crystals. In contrast, mesoporous silica materials provide facile pore accessibility for large alkylate molecules such as 224-TMP, as evidenced by complete desorption of 224-TMP even at mild temperatures. These insights provide guidance for rational engineering of stable solid acid alkylation catalysts.
No takes yet. Share an insight, caveat, or question.
Gong et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: