Hard piezoelectric ceramics of manganese (Mn)-modified 0.36BiScO3–0.64PbTiO3 (0.36BS–0.64PTM) with a high Curie temperature were prepared using the traditional solid-state reaction method. The effects of different concentrations of Mn on the structure, dielectric and piezoelectric properties of the 0.36BS–0.64PTM ceramics were investigated. X-ray diffraction results indicated that the 0.36BS–0.64PTM ceramics showed a single perovskite structure with tetragonal symmetry and the c/a ratio decreased slightly with increasing Mn content. The grain sizes of the 0.36BS–0.64PTM ceramics were enlarged by Mn addition, and their distributions were uniform. The dielectric loss tan δ decreased clearly with the increase in Mn content, and the mechanical quality factor Q m and vibration velocity v 0 were improved significantly at the same time. The Curie temperature T c, the planar electromechanical coupling factor k p, dielectric loss tan δ, mechanical quality factor Q m and vibration velocity v 0 of the 0.36BS–0.64PTM ceramics with 3 mol% Mn were about 431 °C, 0.57, 0.007, 134 and 1.05 m s−1, respectively. The maximum vibration velocity v 0 of the 0.36BS–0.64PTM ceramics is much superior to those of PZT (0.4 m s−1) ceramics and PZT–PZM (0.72 m s−1). These results indicated that the 0.36BS–0.64PTM ceramics are promising candidates for high-temperature and high-power piezoelectric applications.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: