The study dealed with an analysis of the fracture toughness of spruce wood loaded in mode I with respect to loading rate (0.5, 5 and 50 mm/min) and moisture content (11, 17, 19, and 22%). The mode I was applied at the RL plane using a single-edge notch three-point bending (SEN-3PB), fracture parameters were calculated using both direct data and compliance-based beam method (CBBM). The work also compared total fracture energy Gf computed by nominal and real crack surface obtained after the test. Results show that fracture properties are statistically lower for the MC level of 22% compared to other MC levels, and Gf is the most sensitive measure out of the studied ones. The measured critical energy release rate (Gc) was in agreement with the literature and dropped about 31-45% at the MC level 22% when compared to the MC level of 11.5%. Loading rates did not influence any fracture properties at either MC level, which implies that fracture tests using SEN-TPB with loading-rate up to 50 mm/min likely provide valid outputs. Data showed that it is advisable to measure real crack length in the tangential direction since the nominal Gf are overestimated up to 7%.
No takes yet. Share an insight, caveat, or question.
Sebera et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: