The internal photoelectric-effect technique in combination with multiple internal reflection measurements has been used for quantitative measurement of impurities and defect-related traps in the thin Si3N4 insulating film of a metal–nitride–oxide–semiconductor device, and their correlation with film processing conditions. The hydrogen content in the film showed an increase of approximately 3% for a decrease of deposition temperatures from 950 to 700 °C and corresponding increase in trapped electron density from 0.55×1018 to 2.0×1018 cm3. The multiple internal reflection measurements indicated that the variation in the hydrogen content in the Si3N4 film was predominantly related to a variation in hydrogen-to-silicon bonding while the hydrogen bonded to nitrogen was relatively constant. The results suggest that hydrogen, in addition to excess silicon, and perhaps other structural defects, plays a role in determining trapped electron densities in silicon nitride.
No takes yet. Share an insight, caveat, or question.
Kapoor et al. (1983) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: