We have examined the kinetics of low pressure chemical vapor deposition of tungsten by the hydrogen and silicon reduction of WF 6 within a pressure range of 0.1–5 torr and a temperature range of 250°–500°C. The rate‐limiting mechanism for the hydrogen reduction system was determined to be the dissociation of H 2 adsorbed on the surface, with an activation energy of 0.71 eV. A self‐limiting deposit results from the WF 6 ‐ Si reaction, the thickness and structure of which are dependent upon the initial native oxide characteristics. Deposition occurs selectively on materials that react directly with WF 6 or yield monatomic hydrogen. In the presence of hydrogen, the degree of selectivity is a function of temperature, substrate material, and surface cleanliness.