Al2O3 has been shown to provide an outstanding passivation quality on p‐type surfaces after annealing at moderate temperatures (∼425 °C). However, most industrial silicon solar cells are based on printing technologies for metallization, including a high temperature firing step for the contact formation. To investigate the thermal stability of the Al2O3 passivation, symmetrical p and p+ np+ lifetime samples were coated with Al2O3 and exposed to typical firing processes at temperatures between 700 °C and 850 °C. Up to a firing temperature of 825 °C the Al2O3 passivation is shown to be stable on highly boron‐doped surfaces. An emitter saturation current density of ∼60 fA/cm2 could be measured for the p+ np+ samples, allowing a maximum open circuit voltage (Voc) >695 mV. The firing stability of the Al2O3 is an important step for the realization of an industrial n‐type silicon solar cell. (© 2009 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)
No takes yet. Share an insight, caveat, or question.
Benick et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: