The reduction of mercury on a fresh iridium surface is reversible with a half‐wave potential of +162 mV ( vs. SCE). A Hg(O) monolayer is formed by underpotential deposition (UPD) at +600 mV during the initial scans of a repetitive cyclic voltammogram. This monolayer acts as bulk Hg(O) during further cycles, and the reduction half‐wave potential then shifts towards +410 mV. Anodization of the electrode at a potential > +1000 mV returns the reduction wave to its original position. The peak for the oxidation of bulk Hg(O) from the surface occurs at +430 mV followed by a peak for the underpotential stripping (UPS) of the Hg(O) monolayer at +650 mV. The quantity of Hg(O) for the monolayer corresponds to a 40% coverage of the Ir surface. The underpotential shift for the bulk and monolayer stripping of Hg(O) from Ir was found to be 210 mV. No indications of a Hg‐soluble compound formation between Hg and Ir were found.
No takes yet. Share an insight, caveat, or question.
Kounaves et al. (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: