The phase transformation sequence, microstructure and compositions, and magnetic properties for a melt-spun Sm(Co0.68Fe0.2Cu0.1Zr0.02)7.5 alloy after isochronal heat treatments have been studied by using x-ray diffraction, transmission electron microscopy, three-dimensional atom probe (3DAP), and magnetometry. The as-spun ribbons had a single phase with the Cu7Tb structure. After being aged at 720°C, the single phase decomposed into two major phases: 2:17R and 1:5H, and one minor CoFeZr-rich phase. The formation of the Z-phase happened after the cellular structure, requiring a higher temperature than that for the cellular structure. The 3DAP analysis showed that Zr was depleted from the 2:17R and 1:5H phases by a half while the other elements remained almost unchanged when the aging temperature increased from 720to840°C. In contrast to the sintered permanent magnets, Cu was enriched in the 1:5H phase with a much higher concentration (>40at.%). The Cu enrichment also occurred at the boundary of the Z-phase. The coercivity achieved was Hc=4.34kOe following aging at 720°C. The highest maximum energy product, (BH)max, was 6.48MGOe after aging at 800°C and the remanence to saturation magnetization ratio, Mr∕Ms, was 0.69. This relatively low Hc and high Mr∕Ms ratio may be a consequence of the formation of a significant volume fraction of the CoFeZr-rich nanocrystalline phase.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Xiong et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: