Sc 2 O 3 films were deposited by atomic layer deposition (ALD) from a new precursor scandium tris( N , N ′ -diisopropylacetamidinate) and water. The precursor is thermally stable ( 350 ° C ) , volatile, with good reactivity to HF-last silicon. A growth rate of 0.3 Å ∕cycle was obtained at 290 ° C . The films were pure ( C , N < 0.5 atom %) and had a refractive index of 1.8. Reactive ion etching tests on ALD scandia showed an etch rate 18 times slower than ALD hafnia. Electrical measurements showed a high permittivity of ∼ 17 , and a leakage current density of < 3 × 10 − 3 A ∕ cm 2 for an equivalent oxide thickness of 1.8 nm at 1.0 V .