The high-temperature creep behavior of Mg-10Gd-0.4Zr alloys with different initial precipitation states was systematically investigated at 225–300 °C. Four microstructural conditions, namely the as-cast, solution-treated (T4), peak-aged (T6), and over-aged states, were examined. Dislocation pile-up and tangling around the α-Mg + Mg 5 Gd eutectic phases caused local stress concentration, whereas coarse incoherent β precipitates were bypassed through the Orowan mechanism, resulting in weak creep strengthening. In contrast, coherent β′ precipitates effectively impeded dislocation motion and provided the strongest creep-strengthening effect. Consequently, the T6 state alloy containing a high density of intragranular β′ precipitates exhibited the best creep resistance below 260 °C. At 275 and 300 °C, however, the T4 alloy exhibited better creep resistance than the T6 alloy. TEM analysis revealed distinct precipitation evolution behaviors in the T4 and T6 state alloys during creep at 275 °C. Dynamic precipitation produced a relatively high fraction of β′ precipitates in the T4 alloy, whereas pre-existing β′ precipitates in the T6 alloy progressively transformed into semi-coherent β 1 precipitates. The β 1 precipitates impeded dislocation motion but exhibited lower creep-strengthening capability than β′. These results demonstrated that creep resistance was governed by both the initial precipitation state and its temperature-dependent evolution during creep.
No takes yet. Share an insight, caveat, or question.
Qin et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: