Polypropylene (PP) bead foams were prepared by autoclave foaming using n -pentane and CO 2 as the blowing agents. PP foams blown with n -pentane had foaming temperatures of 92–96 °C, expansion ratios of 10–50 times, and a signal T m at 150.1 °C, while PP foams blown with CO 2 had foaming temperatures of 151–153 °C, expansion ratios of 8–20 times, and dual melting peaks at 164.0 and 140.9 °C. Polyethylene (PE) addition was used to improve the foaming behavior of PP and to induce the formation of dual and multiple T m in PP/PE foams. A differential scanning calorimetry procedure was carried out to simulate the steam-chest molding of bead foams. Interbead bonding was found to be determined by the heat of fusion of T mc (crystal melting of the newly formed crystals during fast cooling), Δ H mc . Recrystallization of the PE component contributed to the increase of Δ H mc, which potentially improved interbead bonding of the molded PP/PE bead foams.
No takes yet. Share an insight, caveat, or question.
Lan et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: