Thermal cracking is triggered by frictional thermal shock in high-carbon martensitic steels used as work rolls for cold rolling. However, materials-design strategies that satisfy hardness requirements while mitigating thermal cracking remain underdeveloped. This study proposes a framework linking cryogenic treatment, tempering, retained austenite (RA), hardness, and fracture-related responses in a single material system. AISI 52100 steel was subjected to systematic cryogenic treatment and tempering to produce different RA fractions and associated pre-thermal shock material states while maintaining comparable post-tempering hardness. The quasi-static fracture resistance was evaluated using the critical stress intensity factor, whereas the thermal-crack susceptibility was assessed through frictional thermal-shock testing, microstructural characterization, and residual stress measurements. The quasi-static fracture resistance was primarily governed by hardness and showed limited dependence on the RA fraction. The thermal-crack susceptibility was generally higher in specimens with lower RA fractions. This observation is qualitatively consistent with the contribution from RA-related irreversible-strain accommodation, although other microstructural changes induced by cryogenic treatment may also contribute. The proposed framework provides a conceptual basis for interpreting the roles of hardness, RA fraction, and material states induced by cryogenic treatment and offers guidance for coordinating cryogenic treatment and tempering to mitigate thermal cracking while maintaining the required hardness
No takes yet. Share an insight, caveat, or question.
Ito et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: