Answers are grounded in this paper and cite their sources.
This study presents a comparative evaluation of microwave and ultrasonic joining of kenaf‐reinforced polypropylene composite (KRPC) single‐lap joints and their response to hydrothermal aging. The KRPC specimens were fabricated using microwave‐assisted compression molding. The variation in temperature and pressure during microwave and ultrasonic joining of KRPC single‐lap joints was investigated as a function of joining time. The joined area of the specimens was subjected to hydrothermal aging at 60°C for 17 days until moisture saturation was reached. The microwave‐joined interface was characterized using differential scanning calorimetry, X‐ray diffraction, and Fourier‐transform infrared spectroscopy to analyze thermal, crystallinity, and chemical changes induced by hydrothermal aging at the microwave‐joined lap interface. A specialized fixture was developed to constrain the lap area and prevent bending during the lap‐shear test. The results showed that hydrothermal aging reduced the mechanical performance of the microwave‐ and ultrasonic‐joined KRPC lap joint specimens. The microwave‐joined specimens retained higher absolute mechanical property values after aging, with reductions of 2.06% in lap‐shear strength, 6.78% in impact strength, and 3.69% in three‐point bend failure load, compared with 3.91%, 5.26%, and 4.09%, respectively, for ultrasonic‐joined KRPC specimens.
No takes yet. Share an insight, caveat, or question.
Muliya et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: