Multi‐material fused filament fabrication (FFF) allows hybrid joints to be manufactured in a single uninterrupted process. However, the load‐transfer behavior and failure mechanisms of co‐printed material transitions remain insufficiently understood. This study investigates PLA/PLA‐CF hybrid single‐lap joints manufactured by one‐step FFF with overlap lengths of 8, 12.5, and 25 mm, maintaining constant width and thickness. The results of the quasi‐static tests showed mean maximum apparent lap‐shear stresses of 11.6, 7.9, and 5.3 MPa, respectively. For the 12.5 and 25 mm overlaps, failure occurred in the PLA‐CF adherend. Therefore, the measured apparent stresses represent only lower bounds for the corresponding joint‐region failure limits. In contrast, the 8 mm specimens exhibited cohesive failure within the printed PLA‐CF architecture of the overlap, rather than separation at the PLA/PLA‐CF interface. An adapted Volkersen‐type model was used to examine load transfer based on the observed joint‐region failure and the lower‐bound constraints from the longer overlaps. Three‐dimensional finite element analyses were also performed to evaluate the stress distribution before failure. A preliminary environmental‐economic assessment showed that the preferred configuration depends on the selected mechanical objective, whether maximum specimen load or apparent lap‐shear stress. The manufacturing impacts were also influenced by the adopted specimen geometry.
No takes yet. Share an insight, caveat, or question.
Chairi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: