Answers are grounded in this paper and cite their sources.
This research presents a comparative study of burr width, diametral deviation, and surface roughness (Ra) of blind holes drilled in 7075-T6 aluminum alloy using commercial AISI M2 high-speed steel twist drills, both untreated and selectively borided. The selective boriding thermochemical treatment was applied at 1223 K for 2 and 4 h, and the resulting boride layers were characterized by optical microscopy, X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy-dispersive X-ray spectroscopy (EDS). One drill bit per condition was subjected to a 1200-hole drilling sequence, from which 148 longitudinally sampled holes per completed run (determined via G*Power) were evaluated using descriptive statistics, the Kolmogorov–Smirnov normality test, the Mann–Whitney U test, and Pearson and Spearman correlation analyses. The 4 h test was stopped after 14 holes due to early coating delamination, indicating a potential thickness threshold. Over the 1200-hole drilling sequence, the 2 h selectively borided drill bit exhibited lower mean surface roughness Ra (2.98 µm vs. 14.70 µm) and lower mean diametral deviation (0.010 mm vs. 0.037 mm) than the untreated drill bit, alongside a moderately larger mean burr width (0.076 mm vs. 0.059 mm). Post-test SEM-EDS analysis indicated that adhesion and abrasion were the predominant wear mechanisms.
No takes yet. Share an insight, caveat, or question.
García-Vanegas et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: