The tensile creep behavior of Si/mullite/BSAS-coated, two-dimensional plain-woven SiC/SiC composites was investigated in wet oxygen at 1300 °C under nominal stresses of 120, 160, and 200 MPa. At 120 MPa, no rupture occurred during testing for up to 300 h. In the examined sample, coating cracks extended into the mullite layer, while the Si bond coat remained uncracked and substrate oxidation was limited. At 160 MPa, two samples ruptured after cumulative loading times of 70 and 139 h, while another remained intact after 100 h. Creep rates reaching the order of 10−9 s−1 or higher during the secondary and tertiary stages were associated with severe damage and increased susceptibility to rupture. Penetrating coating cracks provided pathways for wet-oxygen ingress, promoting substrate oxidation and damage to the load-bearing fibers. At 200 MPa, rupture occurred after approximately 5 min with limited oxidation, suggesting a greater contribution from mechanical damage to short-term failure. The internal defect volume fraction increased from 11.16% to 12.95% after 50 h at 160 MPa. These findings highlight the role of coating integrity in environmental protection and the contribution of oxidation-assisted substrate damage to creep rupture.
No takes yet. Share an insight, caveat, or question.
Cao et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: