Post-weld heat treatment (PWHT) was applied to friction stir welded (FSW) 6061-T6 aluminium alloy joints to assess regional microstructural evolution and mechanical-property recovery. The treatment consisted of solution treatment at 520 °C for 1 h, water quenching, and artificial ageing at 170 °C for 7 h. Microstructural characterisation was performed using EBSD and SEM-EDS, while mechanical properties were evaluated through microhardness measurements and tensile testing. PWHT caused grain growth in the heat-affected, thermomechanically affected, and nugget zones (NZs). In the NZs, mean grain size increased from 10.17 to 16.15 μm, the fraction classified as recrystallised increased from 84.8% to 95.8%, and the high-angle grain-boundary fraction increased from 64.1% to 70.2%; KAM decreased from 0.61° to 0.54°. NZ hardness increased from 55–63 to 106–108 HV. Ultimate tensile strength and yield strength increased from 202.3 ± 2.5 to 299.8 ± 2.0 MPa and from 149.8 ± 1.4 to 249.6 ± 1.7 MPa, respectively, while elongation decreased from 13.8 ± 0.4% to 9.5 ± 0.2%. Both conditions fractured in the NZ. These findings show that PWHT restores hardness and strength but does not change the critical fracture region.
No takes yet. Share an insight, caveat, or question.
Hu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: