Fused deposition modeling (FDM) fabricated polyethylene terephthalate glycol (PETG) may have a corrugated surface and voids between the layers, which can restrict performance in sliding contact. In this study, we investigated a low-cost surface engineering process where the tribologically challenging PETG substrate was structurally selected and the protective coating was the self-curing dental polymethyl methacrylate (PMMA). Three levels of each of the four FDM parameters were screened, with three independently printed specimens for each level of the parameter. Three-trial wear indices were analyzed using the original Taguchi smaller-the-better signal-to-noise (S/N) criterion, and factor-level means and sample standard deviations (SDs) were used to summarize the results for tensile strength, Rockwell R hardness (HRR), and inclined-plane static coefficient of friction (COF). The archived measurements were factor-level triplicates as opposed to responses associated with nine simultaneous L9 combinations. Selected PETG specimens were cross-hatched, acetone cleaned, dip-coated, and cured for 48 h. The coating was applied evenly at 0.5 mm on each face, increasing each reduced-section dimension by 1.0 mm in total. The coated condition had a mean maximum load 24.1% greater. Using condition-specific outer-section areas, the calculated tensile strength was 6.9% lower (27.15 ± 0.48 versus 25.29 ± 0.46 MPa), whereas the calculated tensile modulus was 13.8% higher (6.20 ± 0.25 versus 7.05 ± 0.19 MPa). Mean hardness was 44.2% higher (60.0 ± 0.8 versus 86.5 ± 0.7 HRR). The apparent PETG-equivalent wear index, calculated using a common PETG-density normalization due to the inability to separate the lost PMMA and PETG phases, was 50.0% lower ((27.77 ± 3.97) × 10-3 versus (13.88 ± 1.98) × 10-3 mm3 N-1 m-1). Static COF was 2.0% lower (0.1643 ± 0.0005 versus 0.1611 ± 0.0005), although the absolute change was small. The scanning electron microscopy (SEM) images revealed a more continuous coated surface and no large-scale delamination following the short duration abrasive test.
No takes yet. Share an insight, caveat, or question.
Mustafa et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: