Answers are grounded in this paper and cite their sources.
This study investigated ceramizable phenolic composites for service at 800–1200 °C. High-silica fibers were used as reinforcement, while SiC, B4C, glass powder, and montmorillonite formed a multifunctional support–reaction–liquid-phase filler system. Composites containing only glass powder or montmorillonite served as controls. The hybrid system underwent matrix pyrolysis and particle exposure at 800 °C, liquid-phase bridging and skeleton reconstruction at 1000 °C, and glass-phase coalescence with surface densification at 1200 °C. Its image-derived apparent surface porosity decreased from 16.4% to 8.9% and eventually approached zero, while the continuous ceramicized layer thickened from 10–15 µm at 1000 °C to 20–30 µm at 1200 °C. Residual flexural strength increased from 39 MPa at 800 °C to 56 MPa at 1000 °C, then decreased to 44 MPa at 1200 °C, showing that surface densification does not necessarily enhance bulk load-bearing capacity. Montmorillonite alone produced insufficient liquid phase, whereas glass powder alone caused excessive flow and large pores. Their combination better balanced liquid-phase supply, internal bridging, and high-temperature structural retention. A conceptual ‘liquid-phase window’ framework is proposed for filler design and temperature-dependent ceramization control.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: