Binary CrN and VN, and ternary CrVN ceramic coatings were deposited by DC magnetron co-sputtering from single-element targets, with the nitrogen flow (10, 40 and 80 sccm) as the sole variable. XRD showed the binary ceramics to be highly reactive gas flow-sensitive – CrN evolving from a metallic-Cr/Cr 2 N mixture toward cubic CrN, and VN degrading toward a quasi-amorphous state at 80 sccm – whereas the ternary CrVN retained a well-defined FCC structure across the whole range. SEM-EDS showed that all coatings are nitrogen-deficient (N/Me = 0.35–0.68) and that the loss of long-range order in the binaries coincides with oxygen uptake (O/Me up to ≈ 0.8), which the CrVN coatings, grown at the highest metal flux, largely avoid (O/Me ≤ 0.14). Increasing the nitrogen flow softened all systems (CrN hardest, ≈ 15 GPa; VN softest, ≈ 8 GPa; CrVN intermediate). The CrVN coatings combined competitive hardness with by far the best adhesion (Lc3 up to ≈ 9 N vs ≈ 4 N for the binaries), the lowest friction coefficient (≈ 0.45), the most stable, near-neutral open-circuit potential and the slowest development of corrosion products under SO 2 exposure. Linear polarization showed, however, that nobility does not rank the corrosion kinetics: the apparent corrosion current densities of CrVN (≈ 4–6 µA cm −2 ) were comparable to those of CrN, and the lowest value (≈ 1.2 µA cm −2 ) was obtained for the insulating CrN_80 oxynitride. Within each series, the electrical resistivity and the hardness followed the oxygen content of the coatings rather than their Cr/V ratio, and adhesion was highest for the thickest (CrVN) coatings. Co-sputtering Cr and V therefore yields the best balance of hardness, adhesion, friction and electrochemical stability, making CrVN a promising multifunctional protective coating.
No takes yet. Share an insight, caveat, or question.
Crisbasan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: