Answers are grounded in this paper and cite their sources.
This study investigates the corrosion behavior of 13Cr martensitic stainless steel in supercritical CO 2 under coupled factors: temperature (50∼100°C), flow velocity (0.05∼2.0 m/s), and Cl − concentration (30∼240 g/L). Weight loss tests and multiscale characterization (SEM/EDS/XRD/XPS) show a nonlinear corrosion rate response, peaking at 0.0385 mm/a at 80°C. According to NACE SP 0775-2023, all tested conditions yield “slight corrosion” (<0.05 mm/a), confirming the material's suitability for wellbore tubing. Microscopic analysis indicates that the corrosion products consist of crystalline FeCO 3 and an amorphous layer rich in Cr 2 O 3 and Cr(OH) 3. The enrichment of Cr at the interface may contribute to the formation of a barrier layer that could compensate, to some extent, for film defects caused by Cl − penetration or fluid shear stress. In this study, a support vector regression model based on the radial basis function (SVR-RBF) was constructed using 13 experimental datasets. Under leave-one-out cross-validation, the SVR model yielded R 2 = 0.998 and MSE on the order of 10 −7, which were lower than those of the linear and polynomial regression models on the same dataset. The response surfaces generated by the SVR model provide a model-based interpolation of the corrosion behavior of 13Cr stainless steel under the investigated conditions; however, given the limited dataset and the absence of an independent validation set, these results should be regarded as preliminary and can only serve as a reference for corrosion monitoring and risk assessment in CCS projects.
No takes yet. Share an insight, caveat, or question.
Zhao et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: