Iron‐rich physicochemical textile sludge is converted into biochar at 600°C within 4 h under oxidative treatment and modified with 0.0%–3.0% chitosan (CTS) through a crosslinker‐free solvent‐casting route for methyl orange (MO) adsorption. The BET–BJH results show that the pyrolysis process increases the surface area and pore volume from 18.5 m 2 g −1 and 0.07 cm 3 g −1 in the raw sludge to 73.0 m 2 g −1 and 0.19 cm 3 g −1 in the obtained biochar (BC0.0), whereas 3.0%‐CTS incorporation reduces these values to 29.1 m 2 g −1 and 0.11 cm 3 g −1 in BC3.0. The increment of CTS content shifts MO retention from adsorption on the iron‐rich biochar surface to CTS–assisted polymer–mineral binding, thereby enhancing the PSO‐calculated adsorption capacity from 23.6 mg g −1 for BC0.0 to 39.7 mg g −1 for BC3.0. Also, the incorporation of CTS changes the fitting behavior from the Langmuir‐like pattern of BC0.0 to a Freundlich response in the modified biochars caused by the increased surface heterogeneity. Compared with unmodified BC0.0, CTS–modified biochars show matrix‐dependent advantages in real wastewater at specific pH, reflecting the different removal of particulate/colloidal and soluble color fractions. Moreover, BC3.0 retains more than 50% of MO removal through six adsorption–desorption cycles, indicating acceptable regeneration performance.
No takes yet. Share an insight, caveat, or question.
Nguyen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: