Hydrogenated amorphous silicon nitride (a-SiNx:H) films have been prepared by plasma-enchanced chemical-vapor deposition with a mixture of SiH4 and NH3 at a substrate temperature of 250 and 300 °C. The properties of these films have been investigated using x-ray diffraction, infrared absorption, photoluminescence, and electron probe microanalysis. From the x-ray-diffraction measurement, it is found that the short-range order of a-SiNx:H with a basic unit of 4.31 Å appears when the nitrogen-to-silicon ratio in the film exceeds 0.75 at a substrate temperature of 300 °C. In the infrared-absorption measurement, the sample was annealed repeatedly at various temperatures (300–800 °C) to identify the molecular unit responsible for each absorption peak. It is found that part of the infrared-absorption bands between 870 and 1100 cm−1 are caused not by the absorption but by the reflection of infrared radiation due to reststrahlen effect. The absorption peak at 840 cm−1 is assigned to the isolated N in the Si-host network, whereas the peak at 885 cm−1 is assigned to a local bonding arrangement involving a terminal N-H group attached to the amorphous Si network, Si-NH-Si. The transverse optical phonon of crystalline Si3N4 is found to peak at 870 cm−1. Two peaks are observed in photoluminescence experiments when the mole fraction of ammonia in gas phase is smaller than 0.8 indicating the inhomogeneity of the a-SiNx:H films. The higher-energy peak is visible in the red.
No takes yet. Share an insight, caveat, or question.
Lin et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: