Answers are grounded in this paper and cite their sources.
Electron cyclotron resonance plasma-enhanced chemical va- por deposition (ECR-PECVD) is used to deposit thin films of SiN x of different composition from mixtures of N2 and 30% SiH4 in Ar onto dif- ferent substrates. Measured values of the complex refractive index over the wavelength range of interest are used in the design and computer- controlled fabrication of one- and two-band rugate optical interference filters. The excursion of the continuously varying refractive index is cho- sen to be between 0.8 and 1.2, and window functions and matching layers at both sides are employed for sidelobe suppression. Measured reflection patterns of filters agreed well with simulated results. Filters designed for a center wavelength of 1000 nm and a total thickness of 2.1 mm, have a reflectance of 97% in the stopband and a bandwidth of typically 240 nm. The two-band filter is designed for stopbands at 1000 and 770 nm with reflectance of 98 and 96% and bandwidths of 150 and 120 nm, respectively. The total thickness of this filter is 3.33mm. Filters are successfully deposited on optical fiber ends using one of the fibers for in situ monitoring of the deposition process.
No takes yet. Share an insight, caveat, or question.
Pieter L. Swart (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: