The instrument gives an absolute measurement of impurity concentration in a semiconductor wafer as a function of depth and surface position. A matrix of Schottky barrier diodes is deposited on the surface, contact being made with each diode in turn by a small probe. The probe is fed with a dc bias voltage and a small voltage at 100 kHz, the 100 kHz current flowing in the diode being a measure of the small-signal capacitance C x . Another small voltage, at 1 kHz, is superimposed. and the consequent depth of modulation of the 100 kHz current is a measure of dC x /dV. The impurity concentration N and the depth are known functions of C x and dC x /dV, and the instrument does the appropriate analogue computations to provide a direct plot of lg N against depth as the dc reverse-bias voltage is carried. This paper includes a detailed discussion of the sources of error, and also presents some typical impurity profile curves which have been obtained.
No takes yet. Share an insight, caveat, or question.
Baxandall et al. (1971) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: