A cationic surfactant, cetyltrimethylammonium bromide, was used to prepare LaF 3 :Eu 3+ nanocrystals via a hydrothermal route. The influences of post‐annealing temperature on the size and morphology as well as on the photoluminescence (PL) properties were studied. It was found that the PL intensity was maximized when LaF 3 :Eu 3+ nanocrystals were calcined at 600°C. By applying a time‐resolved PL spectral analysis to the 5 D 0 – 7 F 1, 2 decay curves, we could conclude that at the annealing temperature the most of Eu 3+ ions (94.6%) were successfully incorporated in a higher symmetric site in a LaF 3 lattice structure and as a result engaged in the strong PL.