This is the authors' abstract. We don't add key points for this paper.
Crack-free transparent ferroelectric Pb0.865La0.09Zr0.65Ti0.35O3 [PLZT (9/65/35)] thin films have been deposited on silicon substrates using the sol-gel deposition technique. An intermediate layer of Pb0.90La0.10Ti0.975O3 (PLT) was used to improve the PLZT’s optical quality and to reduce the amount of film cracking. Wet chemical etching, plasma etching, and reactive ion etching were investigated as means of realizing the necessary waveguide structures. Waveguiding was observed in 2–4 mm long by 20 μm wide PLZT (9/65/35) ridge waveguides fabricated by reactive ion beam etching.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Baude et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: