This is the authors' abstract. We don't add key points for this paper.
ScN layers, 180 nm thick, were grown on MgO(001) substrates at 750 °C by ultra-high-vacuum reactive magnetron sputter deposition in pure N2 discharges. N/Sc ratios, determined by Rutherford backscattering spectroscopy, were 0.98±0.02. X-ray diffraction θ–2θ scans and pole figures combined with plan-view and cross-sectional transmission electron microscopy showed that the films are strongly textured, both in plane and along the growth direction, and have a columnar microstructure with an average column width near the film surface of 30±5 nm. During nucleation and the early stages of film growth, the layers consist of approximately equal volume fractions of 002- and 111-oriented grains. However, preferred orientation evolves toward a purely 111 texture within ≃40 nm as the 002 grains grow out of existence in a kinetically limited competitive growth mode. 002 grains exhibit local cube-on-cube epitaxy with an orientation relationship (001)ScN∥(001)MgO and [010]ScN∥[010]MgO while 111 grains have a complex fourfold 90°-rotated in-plane preferred orientation in which strained ScN triangular {111} surface unit cells exhibit local epitaxy with square MgO unit cells yielding the orientation relationship (111)ScN∥(001)MgO, [11̄0]ScN∥[11̄0]MgO, and [112̄]ScN∥[110]MgO. Room-temperature electrical resistivity ρ is 1.2×104 μΩ cm while dρ/dT was found to be negative, indicating semiconducting behavior, with ρ varying from 1.6×104μΩ cm at 80 K to 1.1×104 μΩ cm at 400 K. Optical absorption coefficients ranged from 1×104 cm−1 at 1.5 eV to 2.6×105 cm−1 at 3.5 eV with a well-defined edge corresponding to a direct transition at 2.37±0.05 eV.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Gall et al. (1998) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: