Answers are grounded in this paper and cite their sources.
Hexagonal WSi2 was found to form from nearly amorphous cosputtered (tungsten and silicon) mixtures depostied on oxidized silicon. This form of WSi2 was detected in films sintered at temperatures in the range 400–600 °C. At temperatures of 700 °C or above, only tetragonal WSi2 formed. The hexagonal-to-tetragonal transformation temperature was found to be ∼550 °C. At 600 °C the transformation appears to follow a square root of time dependence.
No takes yet. Share an insight, caveat, or question.
Murarka et al. (1981) studied this question.