Two different hydroxyapatites with the particle sizes of 3.9 and 1.69 μm were chosen. Slurries with initial hydroxyapatite concentration of 15 vol% were prepared. Different cooling rates from 2 to 14°C/min were utilized. The specimens were sintered at different temperatures of 1250–1350°C. The phase composition (by X‐Ray Diffraction), microstructure (by Scanning Electron Microscopy), mechanical characteristics, and the porosity of sintered samples were assessed. The porosity of the sintered samples was in range of ~57–83%, and the compressive strength varied from ~1.7 to 15 MPa. The mechanical strength of the scaffolds increased as a function of cooling rate and sintering temperature.