Organic FETs (OFETs) with bilayer dielectric poly(4-vinylphenol) (PVP)/HfO2and polyvinyl alcohol (PVA)/HfO2were fabricated on a flexible low-cost Kapton tape substrate with TIPS -pentacene:polystyrene as an active layer. The devices exhibited average and maximum field-induced mobility of 0.25(±0.10) and 0.37 cm2V-1s-1for PVP/HfO2devices, and 0.35(±0.18) and 0.69 cm2V-1s-1for PVA/HfO2devices, respectively, with low threshold voltage and ION to IOFF ratio approaching 104for both types of devices. Overlapping transfer multiple scans with very less performance variation under ambient conditions were observed. The devices were found to be fairly stable even when electrical stress was applied after a period of 5 months. Devices exhibited small degradation in IDS and small AVTH with high degree of reliability and small performance spreads under combined effects of ambient exposure over a period of 5 months and successive electrical stress. In addition, inverter based on these OFETs with external load was also demonstrated.
No takes yet. Share an insight, caveat, or question.
Raghuwanshi et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: