A new method is developed for the determination of the impurity compensation in n-GaAs on the basis of line-shape analysis of impurity photoluminescence spectra. The observation of these spectra under weak excitation conditions together with a room-temperature free-carrier-concentration measurement enables us to determine the impurity compensation. This method is applied to undoped LPE GaAs crystals with carrier concentrations ranging from 1013 to 5×1015 cm−3. Our method reveals significantly smaller values of the compensation than a conventional mobility analysis. This discrepancy is mainly due to inhomogeneous dopant concentrations in epitaxial layers and the higher spatial resolution of this optical method, provided by the small values of light penetration depth and charge-carrier-diffusion length.