Polycrystalline silicon films of a thickness of 350 nm deposited on a 100 nm thick SiO2 layer are implanted with As+- or P+- ions to dose levels of 5 × 1015, 1016, and 2.5 × 1016 cm−2 at 50 keV and annealed by short light pulses of 10 s duration. The sheet resistivity is investigated as a function of annealing temperature with a systematic study of carrier concentration, electron mobility, impurity redistribution, and grain size. The results are compared to those obtained after conventional furnace annealing for 30 min. Minimum sheet resistivity values obtained after short time annealing are 9 and 18 Ω/□ for P+- and As+-implants, respectively, compared to 11.5 and 40 Ω/□ in conventional annealed samples.