Thermoelectric modules composed of eight pairs of p ‐type Ca 2.7 Bi 0.3 Co 4 O 9 (Co‐349) and n ‐type CaMn 0.98 Mo 0.02 O 3 (Mn‐113) bulks were constructed using Ag electrodes and paste including powder of the n ‐type oxide. The former bulks were prepared by hot pressing. On the other hand, the latter were densified using a cold isostatic pressing technique and sintered in atmospheric pressure. Dimensions of both oxide legs were 5 mm wide and thick and 4.5 mm high. An alumina plate was used as a substrate, and there was no alumina plate on the other side of the modules. When the substrate side was heated, the module could generate up to 1.0 V and 0.17 W of open circuit voltage ( V O ) and maximum power ( P max ), respectively, at a hot‐side temperature of 1273 K (furnace temperature as a heat source) and a cold‐side temperature of 298 K (circulated water temperature) in air. But internal resistance R I reached a value of 1.5 Ω, which is about six times higher than the calculated one from resistivity of both p ‐ and n ‐type bulks. When the substrate side was cooled, V O and P max reached 0.7 V and 0.34 W of V O and P max , respectively, at a furnace temperature of 1273 K.
No takes yet. Share an insight, caveat, or question.
Urata et al. (2007) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: