Experimental study demonstrates optimized freeze granulation produces high-strength lithium titanate pebbles, suggesting enhanced durability and tritium release for fusion reactors.
Lithium titanate (Li 2 TiO 3 ) is being considered as a promising ceramic solid breeder material in the tritium breeding blanket of thermonuclear fusion reactors. This study depicts the fabrication of Li 2 TiO 3 ceramic pebbles by a novel freeze granulation technique followed by freeze‐drying. Prior to the pebble fabrication, optimizing the slurry is a critical step to ensure a well‐dispersed suspension, which is essential for achieving the uniform pore distribution and enhanced crush load in the final Li 2 TiO 3 ceramic pebbles. The rheological study on Li 2 TiO 3 slurry was performed using four different anionic dispersants, namely polyacrylic acid (PAA), maleic acid, Darvan‐C, and BYK‐154 with different concentrations. The effect of solid loading (30–45 wt.%) and binder content (1–7 wt.% polyvinyl alcohol [PVA]) was systematically investigated on pebble castability, microstructure, pore size distribution, and crush load. The effect of sintering temperature (1000°C, 1100°C, and 1200°C) was studied on the properties of the pebbles. Optimal fabrication conditions comprising 40 wt.% solid loading, 7 wt.% binder concentration, and sintering at 1100°C resulted in pebbles with excellent sphericity and a maximum average crush load of ∼83 N. Additionally, a uniform pore distribution in the range of 0.5–7 µm was obtained, which is favourable for efficient tritium release during reactor operation.
No takes yet. Share an insight, caveat, or question.
Kumar et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: