The reliability of determination of model parameters for the Bi2Te3 − x Se x alloys is improved by extending the concentration and temperature ranges in experimental studies and, correspondingly, in calculations of kinetic coefficients based on the two-band model of the electronic spectrum. The obtained results served as a motivation for a study of the thermoelectric figure of merit for the above-mentioned alloys with x = 0.3, 0.45, and 0.6 and with the electron concentration varied in the range (1–50) × 1018 cm−3 at temperatures 300–550 K. Comparison of the results showed that the highest efficiency is exhibited by the Bi2Te2.7Se0.3 alloy with the absolute value of the thermoelectric power of about 165 μVK−1 at 300 K, and the dimensionless efficiency is equal to 1.2 at 410 K. An appreciable decrease in thermal conductivity in alloys with x = 0.6 at 410 K is related to a larger band gap and could beneficially affect the figure of merit. However, the magnitude of this effect is found to be too small to compensate a decrease in electrical conductivity due to a large fraction of heavy electrons in the concentration and to a high content of selenium.
No takes yet. Share an insight, caveat, or question.
Prokofieva et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: